    To improve activation properties and decrease the corrosion rates of aluminum,effects of additives H2O on electrochemical behaviors of aluminum anode(99.999%)in alkaline carbinol-ethanol organic solution were studied by using electrochemical methods.It is shown that corrosion rates of aluminum are largely depressed by 4 mol/L KOH+carbinol-ethanol(5∶5)+30%H2O solution,and corrosion inhibition percentage is 70.04%.At-1.20 V,its current density is 72.66 mA/cm2.Eocp is-1.933 V.

    Reference
    Related
    Cited by
Get Citation
Share
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:
  • Revised:
  • Adopted:
  • Online: November 28,2016
  • Published: