Cure Rheology Characteristics of PBT/N100 Binder System
Author:
Affiliation:

School of Materials Science and Engineering, Beijing Institute of Technology, Beijing 100081

Clc Number:

TJ55

Fund Project:

  • Article
  • |
  • Figures
  • |
  • Metrics
  • |
  • Reference
  • |
  • Related
  • |
  • Cited by
  • |
  • Materials
  • |
  • Comments
    Abstract:

    In order to deeply understand the curing reaction process of 3,3-bis(azidomethyl)oxetane/tetrahydrofuran copolymer (PBT) binder and polyisocyanate curing agent (N100), the modulus changes during the entire isothermal curing process and the viscosity changes before gelation for PBT/N100 binder system was studied by using a rheometer. The results show that the entire isothermal curing process of PBT/N100 binder system follows the autocatalytic kinetic model. According to the change of modulus with curing time, the curing process of PBT/N100 binder system is divided into reaction-control stage, gelation stage and diffusion-control stage. Dual-Arrhenius model can be used to describe the changes of viscosity in the reaction- control stage. The activation energy for viscosity and the activation energy for reaction are 36.271 kJ/mol and 54.882 kJ/mol, respectively. The Eyring model is used to calculate the thermodynamic parameters ΔH and ΔS during the curing process, which are 52.07 kJ/mol and -125.55 J/(mol·K), respectively. It is basically confirmed that the ideal isothermal curing temperature for PBT/N100 binder system is 60 ℃, and the curing time is about 160 h.

    Reference
    Related
    Cited by
Get Citation
Share
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:November 24,2020
  • Revised:December 02,2021
  • Adopted:January 11,2021
  • Online: February 25,2022
  • Published: February 28,2022