    摘要:

    为解决RT-芋环氧类外防热涂料在某产品上出现的裂纹、开裂、脱落等问题,将端羟基聚丁二烯黏合剂
    (HTPB)环氧化,并将其加入到RT-III 环氧类外防热涂料中,提高涂料的延伸率。增韧后涂料RT-IV 的延伸率大幅
    提高,工艺性能有所改善,隔热性能等与增韧前的RT-芋环氧类外防热涂料基本相当,界面性能适当降低,并通过了飞
    行试验验证。通过提高RT-芋环氧类外防热涂料延伸率技术研究,发现在环氧类外防热涂料中适当加入环氧化的端
    羟基聚丁二烯黏合剂(EHTPB),可以达到提高涂料延伸率的目的。

    Abstract:

    To resolve the crack,cracking,fall off and other problems of the epoxy coating,the epoxidized HTPB which
    named EHTPB,was added to the RT-III to improve the elongation of coating. The toughening coating RT-IV not only had a
    good elongation and manufacturability,but also had a good insulation property compared with the RT-III. However,the in鄄
    terfacial property would reduce appropriately. The RT-IV has been verified by the flight experiment. By studying on increas鄄
    ing the elongation of RT-III,it is found that the elongation will be increasing when the EHTPB is added to the coating.

    参考文献
    相似文献
    引证文献
引用本文

刘洪超.环氧类外防热涂料延伸率的提高[J].宇航材料工艺,2012,42(5).

复制
分享
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 最后修改日期:
  • 录用日期:
  • 在线发布日期: 2016-11-28
  • 出版日期:
文章二维码