    Two molding press processes with different cooling methods were adopted to manufacture poly-trifluorochloroethylene (PCTFE) seat sealing ring for ball valve. The results of cryogenic experiments show that internal micro-cracks would occur in the PCTFE product prepared by press process with natural cooling, while the one prepared by press process with pressurized cooling will not generate intrinsic micro-cracks. The results of characterizations and performance tests indicate that molding press process with natural cooling leads to occurrence of micro-cracks in the product, resulting in the subsurface defects during the cryogenic experiments and seal failure. Pressurizing the product during cooling will inhibit the occurrence of micro-cracks,avoiding the appearance of aggravated cracks due to the internal stress generated by the room-low temperature cycle condition.

    Reference
    Related
    Cited by
Get Citation
Share
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:June 18,2020
  • Revised:November 23,2020
  • Adopted:June 26,2020
  • Online: January 15,2021
  • Published: December 30,2020