    摘要:

    用等离子喷涂的方法在不同温度的45#钢基体上制备ZrO2 涂层,通过涂层的结合实验、X 射线衍
    射分析了基体温度与涂层结合强度之间的关系,发现当基体预热温度为250益时涂层的结合强度最高,可达
    13. 4 MPa;当预热温度高于350益时,粘结层中的热生长氧化物明显增加,导致涂层的结合强度降低。

    Abstract:

    ZrO2 coating was developed by plasma spraying process in different substrate preheating temperature, and the tensile test and XRD were used to investigate the influence of substrate preheating temperature on tensile strength. The highest tensile strength can be obtained when the substrate preheating temperature is 250, the highest value is 13.4 MPa.When substrate preheating temperature is higher than 350, the mass of the thermally grown oxide on bond coatings increased more and the tensile strength reduced.

    参考文献
    相似文献
    引证文献
引用本文

王德朋 李庆会 王旭东.基体预热温度对ZrO2 涂层结合强度的影响[J].宇航材料工艺,2010,40(3).

复制
分享
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 最后修改日期:
  • 录用日期:
  • 在线发布日期: 2016-11-28
  • 出版日期:
第十一届航天复合材料成形与加工工艺技术中心交流会 征文通知

关闭