    摘要:

    某管道法兰由镀镍不锈钢管与铝管通过钎焊的方式焊接而成,力学试验过程中钎焊缝部位发生开裂导致泄漏。通过断面形貌观察、能谱及金相分析发现,法兰钎焊焊缝界面处生成了10~20 μm厚的Al-Fe金属间化合物层,分析认为焊缝发生开裂的原因是焊接过程中焊缝界面处反应过度生成了较厚的脆性金属间化合物层,焊接接头偏脆因而试验过程中在试验载荷作用下发生脆性开裂。

    Abstract:

    The pipe flange is made of nickel-plated stainless steel tube and aluminum pipe welded by brazing. In the mechanical test process, the weld seam cracks and leads to leakage. Through morphological observation,energy spectrum analysis and metallographic analysis it is considered that 10 to 20 μm Al-Fe intermetallic layer is found in weld interface,flange welds cracking reason should be the weld interface in the welding process of over reaction,which generates brittle metal thick intermetallic layer, and brittle fracture occurred in the welding joint during the mechanical test.

    参考文献
    相似文献
    引证文献
引用本文

谢国君,王影,韩露.铝/钢法兰钎焊焊缝开裂失效分析[J].宇航材料工艺,2017,47(6):79-82.

复制
分享
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2017-03-16
  • 最后修改日期:2017-06-12
  • 录用日期:
  • 在线发布日期: 2017-12-12
  • 出版日期:
第十一届航天复合材料成形与加工工艺技术中心交流会 征文通知

关闭